ABSTRACT
The aim of this manuscript is to describe 2-year follow-up of a clinical experience with
a zirconia-reinforced lithium silicate ceramic for an anterior rehabilitation with single
metal-free crowns. The maxillary-central incisor teeth crowns were made by zirconiumreinforced lithium silicate and covered with porcelain were obtained with a digital impression with the intra-oral scanner of the CEREC system as a basis for virtual design,
as well as a laminate for the left lateral maxillary incisor, based on a “double scanningâ€
technique. Lithium silicate material seems to be a safe and satisfactory alternative for
anterior crowns’ rehabilitation.
Keywords
Rehabilitation
Aesthetic Dentistry
Dental Ceramics;
Zirconia
Anterior Crowns
Prof. Richard Price, Dr Mohammed AlQahtani, Dr Maan Alshaafi